Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia, Brazil, Chile, Colombia, Mexico, Paraguay, Peru, Uruguay and Venezuela. Voridian PET 9921P will be used primarily for thick wall applications such as refill bottles for water and carbonated soft drinks. Applications/Uses APET and thick sheetBeverage packagingCustom containersThick wall containersBottlesSealing layer for CPET traysRefillable bottles |