MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

3M Scotchkote™ 60FG 534 Urethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Scotchkote Urethane Elastomer 60FG 534 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components.

Product Features:

  • Physical properties similar to factory produced rubbers.
  • Designed for application by brush at thicknesses up to 250 microns
  • Also suitable for molding and casting of flexible components
  • Primarily designed for use to resurface impellers, chutes, and hoppers.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Thickness 254 microns10.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength at Break 6.89 MPa999 psi
Elongation at Break 800 %800 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.0 kV/mm406 kV/in
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hourInitial Set
 960 min16.0 hourMachining Time
 4320 min72.0 hourFull Mechanical
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chesterton ARC 855 Abrasion Control Coating
Chesterton ARC 982 100% Novolac acid resistant coating
Lehvoss LUVOCOM® 1301/GF/30/TF/15 PPS, linear with glass fiber and PTFE
Mearthane Durethane™ S DS-570D Solid Polyurethane Elastomer
BCC Products Kwik Kast BC 8002 Urethane Casting

PMM35303 / 170050

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.