MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 1301/GF/30/TF/15 PPS, linear with glass fiber and PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled

Material Notes: Properties/attributes include: High continuous-use and heat-distortion temperatures. Non flammable. High-strength and stiffness parts with low creep. Improved friction and wear behavior. Emergency (dry) running property. Highly chemically-resistant parts.

Automotive industry, textile-and office machinery, medical- and precision engineering. Typical uses include: Control disks, gear wheels, pump impellers, gear parts for automotive appliances, chip carrier.

Processing: The material does not necessarily have to be predried; when originally sealed containers are used, this process may normally be omitted. Processing temperatures above 360°C may very rapidly cause thermal damage and should therefore be avoided. Post-crystallization may lead to warpage at elevated operating temperatures. This can be counteracted by suitable heat treatment. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.69 g/cc1.69 g/ccISO 1183
Moisture Absorption <= 0.0500 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.0500 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 130 MPa18900 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Modulus of Elasticity 11.0 GPa1600 ksiISO 527-2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Flexural Strain at Break 3.0 %3.0 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1fu
Charpy Impact, Notched 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmIEC 60167
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C13.9 µin/in-°FDIN 53752
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 220 °C428 °FContinuous; UL 746B
 240 °C464 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75-2/A
Vicat Softening Point 240 °C464 °FVST A; DIN ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 320 - 340 °C608 - 644 °F
Zone 1 300 - 320 °C572 - 608 °F
Zone 2 310 - 330 °C590 - 626 °F
Zone 3 320 - 340 °C608 - 644 °F
Melt Temperature 330 °C626 °F
Mold Temperature 150 - 180 °C302 - 356 °F
Drying Temperature  50.0 - 90.0 °C
@Time >=14400 sec
122 - 194 °F
@Time >=4.00 hour
 100 - 140 °C
@Time 7200 - 14400 sec
212 - 284 °F
@Time 2.00 - 4.00 hour
Dehumidifying dryer
 
Descriptive Properties
Colornatural color (beige)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer
Lead-Tin Babbitt Alloy
St. Cloud Natural Zeolite (Clinoptilolite)
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric
Chesterton ARC 982 100% Novolac acid resistant coating

PLUU8868 / 193827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.