MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa MAC-451PG Electroplating PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:
    Features:
  • Excellent balance properties
  • Good impact strength
  • Good processing properties
  • Suit for electro-plating

    Applications:
  • Injection molding
  • Automobile license plate
  • Water tank cover
  • Computer and accessories

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc
@Temperature 23.0 °C
1.10 g/cc
@Temperature 73.4 °F
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Temperature 23.0 °C
0.0050 - 0.0070 in/in
@Temperature 73.4 °F
ASTM D955
Melt Flow 19 g/10 min
@Load 5.00 kg,
Temperature 260 °C
19 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50mm/min; ASTM D638
Elongation at Break >= 40 %>= 40 %50mm/min; ASTM D638
Flexural Strength 75.0 MPa10900 psi2mm/min; ASTM D790
Flexural Modulus 2.20 GPa319 ksi2mm/min; ASTM D790
Izod Impact, Notched 4.50 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
8.43 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.20 mm,
Temperature 23.0 °C
NB
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D257
Dielectric Strength 30.0 kV/mm762 kV/in1.6mm; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
@Thickness 6.40 mm
234 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 6.40 mm
212 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94 HB
@Thickness 1.60 - 3.20 mm
HB
@Thickness 0.0630 - 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 265 °C<= 509 °F
Rear Barrel Temperature 220 - 240 °C428 - 464 °FStart Point: 235°C
Middle Barrel Temperature 220 - 250 °C428 - 482 °FStart Point: 240°C
Front Barrel Temperature 230 - 260 °C446 - 500 °FStart Point: 240°C
Melt Temperature 220 - 240 °C428 - 464 °FStart Point: 235°C
Mold Temperature 60.0 - 90.0 °C140 - 194 °FStart Point: 80°C
Drying Temperature 90.0 - 105 °C
@Time 14400 - 21600 sec
194 - 221 °F
@Time 4.00 - 6.00 hour
Pre-dry
Back Pressure 0.000 - 10.0 MPa0.000 - 1450 psi
 
Descriptive Properties
Injection Speed60-90%
Weather Resistance (delta E)ASTM D4459; 200hr xenon lamp

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa MAC-551 PC/ABS Alloy
Kingfa MAC-501 Modified PC/ABS Alloy
Kingfa MAC-751 HF PC/ABS Alloy
Kingfa MAC-501DY Modified PC/ABS Alloy
Kingfa MAC-751 PC/ABS Alloy

PKINGF057 / 104316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.