MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa MAC-751 PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:
    Features:
  • Excellent balance properties
  • Super high impact strength
  • Good electro-plating properties
  • Good processing properties
  • Good gloss

    Applications:
  • Injection molding
  • Automobile instrument panel
  • Electrical and electronic parts
  • Computer and accessories
  • Household appliance thin wall parts

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc
@Temperature 23.0 °C
1.15 g/cc
@Temperature 73.4 °F
ASTM D792
Water Absorption 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
0.20 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Temperature 23.0 °C
0.0050 - 0.0070 in/in
@Temperature 73.4 °F
ASTM D955
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 260 °C
15 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 116116ASTM D785
Tensile Strength at Break 56.0 MPa8120 psi50mm/min; ASTM D638
Elongation at Break >= 60 %>= 60 %50mm/min; ASTM D638
Flexural Strength 80.0 MPa11600 psi2mm/min; ASTM D790
Flexural Modulus 2.40 GPa348 ksi2mm/min; ASTM D790
Izod Impact, Notched  3.50 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
6.56 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 5.40 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
10.1 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
@Thickness 6.40 mm
259 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
@Thickness 6.40 mm
239 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 265 °C<= 509 °F
Rear Barrel Temperature 220 - 245 °C428 - 473 °FStart Point: 230°C
Middle Barrel Temperature 220 - 250 °C428 - 482 °FStart Point: 235°C
Front Barrel Temperature 230 - 260 °C446 - 500 °FStart Point: 240°C
Melt Temperature 220 - 250 °C428 - 482 °FStart Point: 245°C
Mold Temperature 40.0 - 80.0 °C104 - 176 °FStart Point: 60°C
Drying Temperature 100 - 110 °C
@Time 14400 - 21600 sec
212 - 230 °F
@Time 4.00 - 6.00 hour
Pre-dry
Back Pressure 0.300 - 1.00 MPa43.5 - 145 psi
 
Descriptive Properties
Injection Speed60-90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa MAC-551 PC/ABS Alloy
Kingfa MAC-601 AC PC/ABS Alloy
Kingfa MAC-501 Modified PC/ABS Alloy
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy
Kingfa MAC-451PG Electroplating PC/ABS Alloy

PKINGF067 / 104326

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.