MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Fainplast Compounds PH 75/UV Flexible PVC, Transparent Extrusion
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Transparent

Material Notes: Transparent profiles UV resistant

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.24 g/cc0.0434 - 0.0448 lb/in³ISO R 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73 - 7773 - 77ISO R 868
Tensile Strength at Break 15.0 MPa2180 psiISO R 527
Elongation at Break 320 %320 %ISO R 527
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -30.0 °C-22.0 °FCold Flex; ISO 458/2
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable W9400 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible 90401 Polyvinyl Chloride, Flexible
Fainplast Compounds PMS 96 Flexible PVC, Extrusion
Fainplast Compounds PK 85/N Flexible PVC, Lead Free
Fainplast Compounds GSK 88 Flexible PVC, Injection Molding, Lead Free

PFAIN030 / 80232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.