MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Polystone® E natural PE-LD
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product characteristics:
  • High impact strength
  • Good processing properties
  • High flexibility
Product applications:
  • Orthopedic technology
  • Vacuum forming industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³DIN EN ISO 1183-1
Water Absorption <= 0.10 %<= 0.10 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545DIN EN ISO 868
Tensile Strength, Yield 11.0 MPa1600 psiDIN EN ISO 527
Elongation at Break >= 50 %>= 50 %DIN EN ISO 527
Modulus of Elasticity 0.200 GPa29.0 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 85.0 kJ/m²40.4 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmDIN EN 62631-3-1
Surface Resistance 1.00e+14 ohm1.00e+14 ohmDIN EN 62631-3-2
Dielectric Constant 2.42.4IEC 60250
Dielectric Strength 45.0 kV/mm1140 kV/inIEC 60243
Dissipation Factor 0.00060
@Frequency 1e+6 Hz
0.00060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 - 230 µm/m-°C83.3 - 128 µin/in-°FDIN 53752
Specific Heat Capacity 2.10 J/g-°C0.502 BTU/lb-°FDIN 52612
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 110 °C230 °F
Maximum Service Temperature, Air 60.0 °C140 °Flong term
 90.0 °C194 °Fshort term
Vicat Softening Point 96.0 °C205 °FDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))
Polikim ULPOLEN® 1000 UHMWPE Standard
Röchling LubX® CV Tribological UHMWPE
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer

PROCH9205 / 232908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.