MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling LubX® CV Tribological UHMWPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:
  • Excellent dry-running properties
  • High wear resistance
  • Good machinability
Product applications:
  • Automation
  • Materials handling industry
  • Conveyor technology

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Yield 18.6 MPa2700 psiASTM D638
Elongation at Break >= 250 %>= 250 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 180 µm/m-°C100 µin/in-°FASTM D696
Melting Point 135 °C275 °F
Maximum Service Temperature, Air 82.2 °C180 °F
Deflection Temperature at 1.8 MPa (264 psi) 42.2 °C108 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF NoNo
USDA YesYes
 
Descriptive Properties
ColorMedium Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
Polikim ULPOLEN® 1000 UHMWPE Standard
Beijing Evergrow Resources UHF-R2400 UHMW PE Fiber
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))
Röchling Polystone® E natural PE-LD

PROCH9068 / 232771

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.