MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nylene® Vexel™ B12GF15 SA 15% Glass Reinforced PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Description: Vexel™ B12GF15 SA is a 15% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance.

Information provided by Custom Resins.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 93.1 MPa13500 psiASTM D638
Flexural Modulus 4.83 GPa700 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 227 °C440 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 191 °C375 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Syensqo (Solvay Specialty Polymers) Polidan® T/A-MD Polyethylene, Crosslinked (XLPE)
Mitsubishi Chemical Advanced Materials TIVAR™ 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings
Mitsubishi Chemical Advanced Materials TIVAR™ 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material
Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service

PN6C683 / 54318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.