MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: Description: Superelso® 500 HR (SE 500 HR, "Hydrogen Resistant") is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment operating under sour service condition. It is designed to meet the requirements of NACE Standard MR0175, with a maximum hardness of 22 HRC in the heat-affected zone (HAZ) after post weld heat treatment (PWHT). SE 500 HR is manufactured via the electric furnace with dephosphorisation, ladle refining and vacuum degassing to provide a reproducible, clean steel. The use of special steelmaking practice imparting high steel cleanliness, along with a carefully adapted chemistry and a uniform structure provides SE500 HR with excellent resistance to wet H2S cracking, including SSC, HIC and SOHIC. The low carbon content of SE500 HR limits the HAZ hardness after welding and also improves weldability. This steel displays excellent toughness, with a low transition temperature (-60°C/-76°F). This steel is particularly suitable for pressure equipment in wet hydrogen sulfide service in the offshore oil and gas industry, where its high strength allows significant weight and cost reductions.

Mechanical properties for 50-150 mm plates.

Information provided by manufacturer.

Key Words: EN10028 part 6 P500QL2, ASTM A 533C Cl. 2 (mod.), ASME II Part A SA 533C Cl. 2 (mod.)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 590 - 770 MPa85600 - 112000 psiTypical
Tensile Strength, Yield >= 480 MPa
@Strain 0.2 %
>= 69600 psi
@Strain 0.2 %
Elongation at Break 17 %17 %Typical
Charpy Impact >= 50.0 J
@Temperature >=-60.0 °C
>= 36.9 ft-lb
@Temperature >=-76.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Iron, Fe 95.99 - 100 %95.99 - 100 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.0080 %<= 0.0080 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.0020 %<= 0.0020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel SUPERELSO® 500 Quenched and Tempered High Strength Steel for Pressure Equipment
ASTM A387 Alloy Steel, Grade 22, Class 1
Nylene® Vexel™ B12GF15 SA 15% Glass Reinforced PBT
Mitsubishi Chemical Advanced Materials TIVAR™ 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings
Mitsubishi Chemical Advanced Materials TIVAR™ 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material

NINDUST63 / 17601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.