MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik TEGO® Sorb A 30 Odour absorber
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Sorb A 30 is a highly effective odour absorber based on the zinc salt of ricinoleic acid activated by an amino acid.

Application: TEGO® Sorb A 30 excellent odour absorbing properties makes it suitable for a wide variety of applications.

Properties / Benefits: Odour developed by osmogenes like hydrogen sulfide, mercaptane, thioether, isovaleric acid and ammonia can be effectively controlled during the usage of TEGO® Sorb A 30. TEGO® Sorb A 30 has no bacteriostatic or fungi-static properties and does not interfere with biological systems.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 - 1.14 g/cc0.0401 - 0.0412 lb/in³
pH 10 - 10.510 - 10.510% solution
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn 2.6 - 3.2 %2.6 - 3.2 %
 
Descriptive Properties
Appearanceyellowish liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGO®Sorb Conc. 50
Evonik TEGO® Sorb B 80
Sandvik 20C Shock Absorber Strip Steel
Parker Chomerics CHO-MUTE 9005 Microwave Absorber
Hong Kun Group UV 360 UV Absorber

PEVONIL565 / 196769

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.