MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 20C Shock Absorber Strip Steel
Categories: Metal; Ferrous Metal; Special-Purpose Steel

Material Notes: The characteristics of Sandvik 20C shock absorber steel are:
  • High strength and wear resistance
  • High fatigue strength under bending and impact stress
  • Excellent surface finish
  • Low level of non-metallic inclusions
  • Good dimensional tolerances
  • Good flatness
  • Information provided by Sandvik

    ASTM 1095

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.80 g/cc0.282 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate  1750 MPa
    @Diameter 0.475 - 0.600 mm
    254000 psi
    @Diameter 0.0187 - 0.0236 in
     1800 MPa
    @Diameter 0.425 - 0.475 mm
    261000 psi
    @Diameter 0.0167 - 0.0187 in
     1850 MPa
    @Diameter 0.375 - 0.425 mm
    268000 psi
    @Diameter 0.0148 - 0.0167 in
     1900 MPa
    @Diameter 0.275 - 0.375 mm
    276000 psi
    @Diameter 0.0108 - 0.0148 in
     1950 MPa
    @Diameter 0.225 - 0.275 mm
    283000 psi
    @Diameter 0.00886 - 0.0108 in
     2000 MPa
    @Diameter 0.175 - 0.225 mm
    290000 psi
    @Diameter 0.00689 - 0.00886 in
     2050 MPa
    @Diameter 0.125 - 0.175 mm
    297000 psi
    @Diameter 0.00492 - 0.00689 in
     2100 MPa
    @Diameter <=0.125 mm
    305000 psi
    @Diameter <=0.00492 in
    Modulus of Elasticity 210 GPa30500 ksi
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  10.5 µm/m-°C
    @Temperature 30.0 - 100 °C
    5.83 µin/in-°F
    @Temperature 86.0 - 212 °F
     11.5 µm/m-°C
    @Temperature 30.0 - 200 °C
    6.39 µin/in-°F
    @Temperature 86.0 - 392 °F
     12.5 µm/m-°C
    @Temperature 30.0 - 300 °C
    6.94 µin/in-°F
    @Temperature 86.0 - 572 °F
    Specific Heat Capacity 0.460 J/g-°C
    @Temperature 50.0 - 100 °C
    0.110 BTU/lb-°F
    @Temperature 122 - 212 °F
    Thermal Conductivity 49.0 W/m-K
    @Temperature 20.0 °C
    340 BTU-in/hr-ft²-°F
    @Temperature 68.0 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 1.0 %1.0 %
    Chromium, Cr 0.20 %0.20 %
    Iron, Fe 98.1 %98.1 %As Balance
    Manganese, Mn 0.40 %0.40 %
    Phosphorus, P <= 0.020 %<= 0.020 %
    Silicon, Si 0.30 %0.30 %
    Sulfur, S <= 0.010 %<= 0.010 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Sandvik 20C Strip Steel
    Zinc Alloy 7; AG40B; Zn-4Al-0.015Mg; Zamak7
    Zinc AC41A Alloy (Zamak 5), As Cast
    AISI 81B45 Steel
    AISI 1005 Steel

    NSANDV284 / 19178

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.