MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borpact™ SG910MO Polypropylene for Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borpact™ SG910MO is a high impact and transparent polypropylene. This grade provides high gloss, high transparency and excellent impact properties. Applications: containers and products with medium to long flow length, houseware goods with high impact and transparency at ambient and low temperatures, transparent storage crates and boxes (House wares), transparent crates and boxes for industrial handling systems, transparent packaging where high impact is needed (i.e. pails), and technical articles where transparency and impact is needed (i.e. covers).

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm0.010 - 0.020 in/in
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6767ISO 2039-2
Tensile Strength, Yield 23.0 MPa3340 psiISO 527-2
Elongation at Yield 14 %14 %ISO 527-2
Tensile Modulus 0.900 GPa131 ksiISO 527-2
Charpy Impact, Notched  0.200 J/cm²
@Temperature -10.0 °C
0.952 ft-lb/in²
@Temperature 14.0 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature 0.000 °C
1.90 ft-lb/in²
@Temperature 32.0 °F
ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy  5.00 J
@Temperature -10.0 °C
3.69 ft-lb
@Temperature 14.0 °F
ISO 6603-2
 20.0 J
@Temperature 0.000 °C
14.8 ft-lb
@Temperature 32.0 °F
ISO 6603-2
 35.0 J
@Temperature 23.0 °C
25.8 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C162 °FISO 75-2
 
Optical PropertiesMetricEnglishComments
Haze 21 %
@Thickness 1.00 mm
21 %
@Thickness 0.0394 in
plaque; Borealis Method
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa2900 - 7250 psi
 
Descriptive Properties
Injection Velocityhigh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Bamberger Polymers Bapolene® 4062 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4072 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene

PBOREA382 / 108641

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.