MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Features:
  • medium viscosity
  • excellent processability
  • good stiffness
  • environmental stress crack resistance
  • heat performance
  • minimal odor and taste
Applications:
  • closures
  • small appliances
  • housewares
  • toys
  • contains a unique combination of stabilizers

Former A-Top Polymers product; part of Amco product line since 2013.

Key Words: FDA 21CFR177.1520
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.906 g/cc0.0327 lb/in³ASTM D1505
Melt Index of Compound 12 g/10 min
@Temperature 230 °C
12 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Tensile Strength, Yield 37.6 MPa5450 psi50 mm/min; ASTM D638
Elongation at Yield 8.0 %8.0 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1550 MPa225000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.374 J/cm
@Temperature 22.8 °C
0.700 ft-lb/in
@Temperature 73.0 °F
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 101L BKB009 PA66
A. Schulman Lucent GPP-120 Polypropylene Homopolymer, 20% Glass Fiber Reinforced, Chemically Coupled
A. Schulman Lucent CPP-120 Polypropylene Homopolymer, 20% Calcium Carbonate Filled
A. Schulman Lucent TPP-120 Polypropylene, Homopolymer, 20% Talc Filled
Celanese Zytel® 101 NC010 PA66

PATOP021 / 79964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.