MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bayport Polymers Baystar™ 9458 HDPE Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.

Applications: Release liners, Stand-up bags, Coextruded films, Shipping sacks, Multi-walled liners, Oriented film structures, Specialty packaging.

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Key Words: Excellent bubble stability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc0.0346 lb/in³ASTM D-792
Water Vapor Transmission 10.9 g/m²/day
@Temperature 37.8 °C
0.700 g/100 in²/day
@Temperature 100 °F
ASTM F1249
Thickness 25.4 microns1.00 milas tested; 2.5 BUR
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 31.0 MPa4500 psiASTM D-882, A
Film Tensile Strength at Yield, TD 17.9 MPa2600 psiASTM D-882, A
Film Elongation at Break, MD 270 %270 %ASTM D-882, A
Film Elongation at Break, TD <= 10 %<= 10 %ASTM D-882, A
Elmendorf Tear Strength MD 15 g15 gASTM D1922
Elmendorf Tear Strength TD 1050 g1050 gASTM D1922
Dart Drop Test <= 50.0 g<= 0.110 lbASTM D1709, A
Film Tensile Strength at Break, MD 53.1 MPa7700 psiASTM D-882, A
Film Tensile Strength at Break, TD 17.9 MPa2600 psiASTM D-882, A
1% Secant Modulus, MD 1070 MPa155000 psiASTM D-882, A
1% Secant Modulus, TD 1370 MPa199000 psiASTM D-882, A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin
ExxonMobil LD 317.87 Film Resin
ExxonMobil HD 7845.30 High Density Polyethylene Resin
ExxonMobil Exceed™ 1318CA Blown Film Resin
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin

PBAYST812 / 177710

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.