MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LD 02519.LQ Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LExxonMobil™ LD 02519.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications. It combines excellent strength properties with outstanding processability.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 4000 ppm
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Agricultural Film
  • Blend Partner
  • Collation Shrink
  • Construction Film
  • Heavy Duty Bags
  • Pallet Shrink Film
  • Zipper Bag

Information provided by ExxonMobil

Key Words: LDPE LD 051.LQ
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ExxonMobil method
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 4000 ppm4000 ppm
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 53.4 N12.0 lb (f)
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa1500 psiASTM D882
Film Elongation at Break, MD 130 %130 %ASTM D882
Film Elongation at Break, TD 570 %570 %ASTM D882
Puncture Energy 8.41 J6.20 ft-lb
Elmendorf Tear Strength MD 340 g340 gASTM D1922
Elmendorf Tear Strength TD 120 g120 gASTM D1922
Dart Drop Test 190 g0.419 lbASTM D1709A
Film Tensile Strength at Break, MD 25.5 MPa3700 psiASTM D882
Film Tensile Strength at Break, TD 21.4 MPa3100 psiASTM D882
1% Secant Modulus, MD 186 MPa27000 psiASTM D882
1% Secant Modulus, TD 241 MPa35000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 110 °C<= 230 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 20 %20 %ASTM D1003
Gloss 33 %33 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 5805 High Density Polyethylene Resin
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Baystar™ 9458 Medium Molecular Weight High Density Polyethylene Film Resin
Braskem F7018 LDPE Injection Molding Polyethylene

PEX99201 / 175437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.