MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Xyron® NC42Z Modified Polyphenylene Ether  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa Parts, Impellers, Valve Bodies, Electrical Base Pans, Fuse Box Components, Control Boxes, Electrical Boxes, Battery Cases

Information provided by Asahi Kasei

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/cc
Filler Content 20 %20 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 78.0 MPa11300 psi
Flexural Modulus 3.50 GPa508 ksi
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM 3.2mm
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °F
Flammability, UL94 5VA5VA5VA

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Xyron™ 1950J PPE/PS, Flame Retardant
Asahi Kasei Xyron™ 240Z PPE/PS, Flame Retardant
Asahi Kasei Xyron® 450H Modified Polyphenylene Ether
Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether
Asahi Kasei Xyron® X0700 Modified Polyphenylene Ether

PASAHI090 / 24701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.