MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Automotive

Information provided by Asahi Kasei

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Moisture Absorption 0.0900 %0.0900 %23°C, 50% RH 24 hours; ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.0 MPa6240 psi23°C, 50% RH; ASTM D638
Elongation at Break 70 %70 %23°C, 50% RH; ASTM D638
Flexural Strength 60.0 MPa8700 psi23°C, 50% RH; ASTM D790
Flexural Modulus 1.92 GPa278 ksi23°C, 50% RH; ASTM D790
Izod Impact, Notched 2.94 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
5.51 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.0 µm/m-°C
@Temperature -30.0 - 60.0 °C
41.7 µin/in-°F
@Temperature -22.0 - 140 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 113 °C235 °FASTM D648
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Equivalent
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Equivalent
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 290 °C464 - 554 °FResin Temperature
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 90.0 - 100 °C194 - 212 °FPre-drying Temperature
Dry Time 2 - 4 hour2 - 4 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Xyron® A1400 PPE/PA
Asahi Kasei Xyron® X9653 Modified Polyphenylene Ether
Asahi Kasei Xyron® 300Z Modified Polyphenylene Ether
Asahi Kasei Xyron® 300V Modified Polyphenylene Ether
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether

PASAHI071 / 24682

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.