MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Seals Eastern 5723 Fluorocarbon-Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Formulated Viton®. General service.

Information provided by Seals Eastern, Inc.

Key Words: FKM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.92 g/cc1.92 g/ccASTM D297, 15
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 70>= 70ASTM D2240, Type A
 8080AVG; ASTM D2240, Type A
 79
@Treatment Temp. 200 °C,
Time 252000 sec
79
@Treatment Temp. 392 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
 79
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
79
@Treatment Temp. 392 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
 79
@Treatment Temp. 200 °C,
Time 3.60e+6 sec
79
@Treatment Temp. 392 °F,
Time 1000 hour
After Dry Heat Aging; ASTM D865
 81
@Treatment Temp. 200 °C,
Time 605000 sec
81
@Treatment Temp. 392 °F,
Time 168 hour
After Dry Heat Aging; ASTM D865
Tensile Strength at Break >= 10.71 MPa>= 1554 psiASTM D412 Method A
 16.85 MPa2444 psiAVG; ASTM D412 Method A
 12.98 MPa
@Treatment Temp. 200 °C,
Time 360000 sec
1882 psi
@Treatment Temp. 392 °F,
Time 100 hour
After Dry Heat Aging; ASTM D865
 14.83 MPa
@Treatment Temp. 200 °C,
Time 605000 sec
2151 psi
@Treatment Temp. 392 °F,
Time 168 hour
After Dry Heat Aging; ASTM D865
 14.83 MPa
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
2151 psi
@Treatment Temp. 392 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
 15.33 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
2224 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
Tensile Stress at Strain  >= 1.90 MPa
@Strain 50 %
>= 275 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 2.30 MPa
@Strain 25 %
333 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 3.02 MPa
@Strain 100 %
>= 438 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 3.34 MPa
@Strain 50 %
484 psi
@Strain 50 %
Average; ASTM D412 Method A
 5.78 MPa
@Strain 100 %
839 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 181 %>= 181 %ASTM D412 Method A
 317 %317 %AVG; ASTM D412 Method A
 412 %
@Treatment Temp. 200 °C,
Time 605000 sec
412 %
@Treatment Temp. 392 °F,
Time 168 hour
After Dry Heat Aging; ASTM D865
 415 %
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
415 %
@Treatment Temp. 392 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
 437.5 %
@Treatment Temp. 200 °C,
Time 252000 sec
437.5 %
@Treatment Temp. 392 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
 456.5 %
@Treatment Temp. 200 °C,
Time 360000 sec
456.5 %
@Treatment Temp. 392 °F,
Time 100 hour
After Dry Heat Aging; ASTM D865
Modulus of Elasticity 0.01590 GPa2.306 ksiASTM D412 Method A
Poissons Ratio 0.500.50Calculated
Shear Modulus 0.00530 GPa0.769 ksiASTM D412 Method A
Secant Modulus 0.01495 GPa2.168 ksiASTM D412 Method A
Tear Strength Test 215215(psi); ASTM D624, Die B
Compression Set  56 %
@Temperature 200 °C,
Time 79200 sec
56 %
@Temperature 392 °F,
Time 22.0 hour
ASTM D395, Test B
 82 %
@Temperature 200 °C,
Time 252000 sec
82 %
@Temperature 392 °F,
Time 70.0 hour
ASTM D395, Test B
 91 %
@Temperature 200 °C,
Time 1.21e+6 sec
91 %
@Temperature 392 °F,
Time 336 hour
ASTM D395, Test B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °FASTM D1329
Glass Transition Temp, Tg -20.0 °C-4.00 °FASTM D1329
 
Processing PropertiesMetricEnglishComments
Shelf Life 180 Month180 MonthASTM D395, Test B
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 5725 Fluorocarbon-Elastomer
Trelleborg E666 EPDM Rubber
Trelleborg T621 Butyl Rubber
Seals Eastern 5722 Fluorocarbon-Elastomer
Seals Eastern 5724 Fluorocarbon-Elastomer

PSEAL32 / 80179

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.