MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Seals Eastern 5723 Fluorocarbon-Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Formulated Viton®. General service.

Information provided by Seals Eastern, Inc.

Key Words: FKM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.92 g/ccASTM D297, 15
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 70ASTM D2240, Type A
 80AVG; ASTM D2240, Type A
 79
@Treatment Temp. 200 °C,
Time 252000 sec
After Dry Heat Aging; ASTM D865
 79
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
After Dry Heat Aging; ASTM D865
 79
@Treatment Temp. 200 °C,
Time 3.60e+6 sec
After Dry Heat Aging; ASTM D865
 81
@Treatment Temp. 200 °C,
Time 605000 sec
After Dry Heat Aging; ASTM D865
Tensile Strength at Break >= 1554 psiASTM D412 Method A
 2444 psiAVG; ASTM D412 Method A
 1882 psi
@Treatment Temp. 200 °C,
Time 360000 sec
After Dry Heat Aging; ASTM D865
 2151 psi
@Treatment Temp. 200 °C,
Time 605000 sec
After Dry Heat Aging; ASTM D865
 2151 psi
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
After Dry Heat Aging; ASTM D865
 2224 psi
@Treatment Temp. 200 °C,
Time 252000 sec
After Dry Heat Aging; ASTM D865
Tensile Stress at Strain >= 275 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 333 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 438 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 484 psi
@Strain 50 %
Average; ASTM D412 Method A
 839 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 181 %ASTM D412 Method A
 317 %AVG; ASTM D412 Method A
 412 %
@Treatment Temp. 200 °C,
Time 605000 sec
After Dry Heat Aging; ASTM D865
 415 %
@Treatment Temp. 200 °C,
Time 1.21e+6 sec
After Dry Heat Aging; ASTM D865
 437.5 %
@Treatment Temp. 200 °C,
Time 252000 sec
After Dry Heat Aging; ASTM D865
 456.5 %
@Treatment Temp. 200 °C,
Time 360000 sec
After Dry Heat Aging; ASTM D865
Modulus of Elasticity 2.306 ksiASTM D412 Method A
Poissons Ratio 0.50Calculated
Shear Modulus 0.769 ksiASTM D412 Method A
Secant Modulus 2.168 ksiASTM D412 Method A
Tear Strength Test 215(psi); ASTM D624, Die B
Compression Set 56 %
@Temperature 200 °C,
Time 79200 sec
ASTM D395, Test B
 82 %
@Temperature 200 °C,
Time 252000 sec
ASTM D395, Test B
 91 %
@Temperature 200 °C,
Time 1.21e+6 sec
ASTM D395, Test B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °FASTM D1329
Glass Transition Temp, Tg -4.00 °FASTM D1329
 
Processing PropertiesOriginal ValueComments
Shelf Life 180 MonthASTM D395, Test B
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Seals Eastern 5725 Fluorocarbon-Elastomer
Trelleborg E666 EPDM Rubber
Trelleborg T621 Butyl Rubber
Seals Eastern 5722 Fluorocarbon-Elastomer
Seals Eastern 5724 Fluorocarbon-Elastomer

PSEAL32 / 80179

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.