MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen CRP 100 RT BLACK High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Hostalen CRP 100 RT black is a high density polyethylene (HDPE), black colored similar RAL 9004, with high melt viscosity for extrusion, injection and compression molding. The product is used in pipe and sheet applications and provides good stress crack resistance properties (ESCR) combined with very good long term hydrostatic strength even at raised temperature (RT). It has an excellent heat ageing and extremely high extraction stability. Hostalen CRP 100 RT black has a minimum required strength (MRS) classification of 10 MPa and is thereby designated PE 100 according to ISO 12162:2009. Applications: Conduit, Drinking Water Pipe, Industrial, Soil & Waste Pipe

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ISO 1183-1
Oxidative Induction Time (OIT) 40 min
@Temperature 210 °C
40 min
@Temperature 410 °F
ISO 11357-6
Carbon Black Loading 2.25 %2.25 %ISO 6964
Melt Flow  0.45 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.45 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 9.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.5 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 59
@Time 3.00 sec
59
@Time 0.000833 hour
ISO 868
Tensile Strength, Yield 22.0 MPa3190 psi50mm/min; ISO 527-1,-2
Elongation at Break >= 350 %>= 350 %ISO 527-1,-2
Elongation at Yield 8.0 %8.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 1.05 GPa152 ksiISO 527-1,-2
Flexural Modulus 0.300 GPa43.5 ksicreep, 4 point loading/ 2000 hr; DIN 16841
 0.470 GPa68.2 ksicreep, 4 point loading/ 24 hr; DIN 16841
 1.00 GPa145 ksicreep, 4 point loading/1 min; DIN 16841
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1/1eA
 2.40 J/cm²
@Temperature 23.0 °C
11.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
Tensile Creep Modulus, 1 hour 640 MPa
@Pressure 2.00 MPa
92800 psi
@Pressure 290 psi
ISO 899-1
Tensile Creep Modulus, 1000 hours 300 MPa
@Pressure 2.00 MPa
43500 psi
@Pressure 290 psi
ISO 899-1
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 70.0 °C158 °FB50; ISO 306
 
Descriptive Properties
FNCT (hrs)350ISO 16770, 4.0 MPa, 2% Arkopal N100, 80°C
MRS Classification (MPA)10ISO 9080
Processing Methodpipe, sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
LyondellBasell Hostalen 4731B High Density Polyethylene (HDPE), Extruded
Overview of materials for Epoxy, Cast, Unreinforced
Versalis Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin

PEQT8470 / 220105

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.