MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EN S275JR High Manganese, Structural, Hot Rolled, Base Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Key Words: EN 10025(90)A1(93) S275JR. Similar to ASTM 1518, UNS G15180
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³Estimated by MatWeb from similar grade
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  380 - 540 MPa
@Thickness 200 - 250 mm
55100 - 78300 psi
@Thickness 7.87 - 9.84 in
 410 - 560 MPa
@Thickness 63.0 - 80.0 mm
59500 - 81200 psi
@Thickness 2.48 - 3.15 in
 410 - 560 MPa
@Thickness 3.00 - 16.0 mm
59500 - 81200 psi
@Thickness 0.118 - 0.630 in
 430 - 580 MPa
@Thickness <=1.00 mm
62400 - 84100 psi
@Thickness <=0.0394 in
Tensile Strength, Yield  205 MPa
@Thickness 200 - 250 mm
29700 psi
@Thickness 7.87 - 9.84 in
 245 MPa
@Thickness 63.0 - 80.0 mm
35500 psi
@Thickness 2.48 - 3.15 in
 275 MPa
@Thickness <=1.00 mm
39900 psi
@Thickness <=0.0394 in
 275 MPa
@Thickness 3.00 - 16.0 mm
39900 psi
@Thickness 0.118 - 0.630 in
Elongation at Break  12 %
@Thickness <=1.00 mm
12 %
@Thickness <=0.0394 in
Transverse
 14 %
@Thickness <=1.00 mm
14 %
@Thickness <=0.0394 in
Longitudinal
 17 %
@Thickness 200 - 250 mm
17 %
@Thickness 7.87 - 9.84 in
Longitudinal
 17 %
@Thickness 200 - 250 mm
17 %
@Thickness 7.87 - 9.84 in
Transverse
 18 %
@Thickness 63.0 - 80.0 mm
18 %
@Thickness 2.48 - 3.15 in
Transverse
 20 %
@Thickness 63.0 - 80.0 mm
20 %
@Thickness 2.48 - 3.15 in
Longitudinal
 20 %
@Thickness 3.00 - 16.0 mm
20 %
@Thickness 0.118 - 0.630 in
Transverse
 22 %
@Thickness 3.00 - 16.0 mm
22 %
@Thickness 0.118 - 0.630 in
Longitudinal
Modulus of Elasticity 200 GPa29000 ksiEstimated by MatWeb from similar grade
Poissons Ratio 0.290.29Estimated by MatWeb from similar grade
Shear Modulus 80.0 GPa11600 ksiEstimated by MatWeb from similar grade
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmEstimated by MatWeb from similar grade
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FEstimated by MatWeb from similar grade
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FEstimated by MatWeb from similar grade
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FEstimated by MatWeb from similar grade
 
Component Elements PropertiesMetricEnglishComments
Carbon, C  <= 0.21 %
@Thickness <=16.0 mm
<= 0.21 %
@Thickness <=0.630 in
 <= 0.22 %
@Thickness >=63.0 mm
<= 0.22 %
@Thickness >=2.48 in
Iron, Fe >= 98.2 %>= 98.2 %
Manganese, Mn <= 1.5 %<= 1.5 %
Nitrogen, N <= 0.0090 %<= 0.0090 %N max n/a if Al >= 0.020
Phosphorus, P <= 0.045 %<= 0.045 %
Sulfur, S <= 0.045 %<= 0.045 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovako S275JR SB1412 Steel, +AR
ASTM A516 Carbon Steel, Grade 70
EN S355JR High Manganese, Structural, Hot Rolled, Base Steel
ASTM A36 Steel, plate
AISI 1005 Steel

M9ZES275JR / 233257

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.