MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1201-90A  Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 10% - 90 Shore A  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes: Glass Fiber 10% - 90 Shore A

Comments:

  • Glass Fiber
  • 90-A Durometer

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
Filler Content 10 %10 %
Water Absorption 0.40 %0.40 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage  0.0010 cm/cm
@Thickness 3.17 mm
0.0010 in/in
@Thickness 0.125 in
ASTM D955
 0.0010 cm/cm
@Thickness 6.35 mm
0.0010 in/in
@Thickness 0.250 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Tensile Strength, Ultimate 17.2 MPa2500 psiASTM D412
Elongation at Break >= 10 %>= 10 %ASTM D412
Modulus of Elasticity 0.552 GPa80.0 ksiASTM D412
Flexural Yield Strength 15.9 MPa2300 psiASTM D790
Flexural Modulus 0.379 GPa55.0 ksiASTM D790
Compressive Yield Strength 10.3 MPa1500 psiASTM D695
Izod Impact, Notched 6.41 J/cm
@Thickness 3.17 mm
12.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 13.3 J/cm
@Thickness 3.17 mm
25.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmASTM D257
Dielectric Constant 4.8
@Frequency 1e+6 Hz
4.8
@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 15.0 kV/mm380 kV/inS/T; ASTM D149
Dissipation Factor 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
Dry; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 126 µm/m-°C
@Temperature 20.0 °C
70.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.403 W/m-K2.80 BTU-in/hr-ft²-°FThrough-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C130 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
Per testing by RTP Company; ASTM D635
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 210 °C320 - 410 °F
Mold Temperature 37.8 - 60.0 °C100 - 140 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Norton® FEP Fluoropolymer Film
RTP Company RTP 1200.5-90A  Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 5% - 90 Shore A
Chemours 100 FEP Fluorinated Ethylene Propylene
Overview of materials for Vinyl Ester Sheet Molding Compound
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced

PR4616 / 63940

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.