MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Silres® BS 38 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS 38 is a solvent-based mixture of silane, siloxane and fluoropolymer (< C8). In diluted form, it serves to render inorganic substrates such as mineral construction materials water-repellent and oil-repellent. Unlike conventional impregnating agents, which display only a hydrophobic, i. e. water-repellent, effect, SILRES® BS 38 also exhibits an oleophobic, i. e. oilrepellent, effect. The pores of the substrate remain open, the water vapour diffusion is hardly affected, if at all. Oil, grease and paint, etc. can be more easily removed from surfaces that have been treated with SILRES® BS 38.

Application:

  • Treatment of facades of natural or synthetic stone, concrete, or fibrous cement in order to allow easier removal of dirt, grease, graffiti, posters, etc. from monuments, exterior and interior walls.
  • Water, oil and dirt repellent treatment of low-porosity natural stone, e. g. marble, travertine and granite.
  • Treatment of floors of natural or synthetic stone, or unglazed ceramic tiles for easy care.
  • Treatment of window sills and table tops of natural or synthetic stone, or fibrous cement to avoid staining.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc
@Pressure 0.1013 MPa
0.0318 lb/in³
@Pressure 14.69 psi
DIN 51757
 
Thermal PropertiesMetricEnglishComments
Flash Point 43.0 °C109 °FISO 3679
 
Descriptive Properties
Appearanceyellowish
Content (%)46Silane/siloxane/polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Wacker® Silane IO-TRIMETHOXY
Tetrafluorosilane, SiF4
NuSil MED-1055 Silicone, One Part Adhesive/Sealant - Restricted Medical Use
Difluorosilane, SiH2F2
Dichlorodifluorosilane, SiCl2F2

PWACK9535 / 205064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.