MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wall Colmonoy COLMONOY® 226 Custom Formulated Nickel-Based Alloy For Glass
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts such as clutch components.

Method of Application: Fusewelder

Information provided by Wall Colmonoy Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.58 g/cc0.310 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 16 - 2116 - 21
 
Thermal PropertiesMetricEnglishComments
Melting Point 935.0 °C1715 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wall Colmonoy COLMONOY® 227 Custom Formulated Nickel-Based Alloy For Glass
Wall Colmonoy COLMONOY® 228 Custom Formulated Nickel-Based Alloy For Glass
Wall Colmonoy COLMONOY® 225 Custom Formulated Nickel-Based Alloy For Glass
Wall Colmonoy COLMONOY® 21A PTA Nickel Alloy with Tungsten Carbide
Wall Colmonoy COLMONOY® 42 SA Hard Nickel-Chromium-Boron Alloy Containing Chromium Carbides

NWALL28 / 19795

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.