Contains chromium for resistance to wear and sulfur-containing media. Used as cushion for harder overlays such as Colmonoy 56 PTA. Applications: Used primarily on glass container molds and related parts, to fill in defects and worn areas. Information provided by Wall Colmonoy Corporation. |