MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Latrobe HS-29XL™ ASTM M2-HC High Speed Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: HS-29XL (M2-HC) is the M2 composition with the carbon content increased and with the addition of alloy sulfides. The higher carbon content provides higher hardness and superior red hardness compared to standard-carbon M2. The alloy sulfides improve machinability and grindability and make it possible to produce accurately-machined tools without grinding after hardening. Because of the increased carbon content and higher attainable hardness, HS-29XL exhibits abrasion resistance that is similar to M3-1 high speed steel.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.14 g/cc8.14 g/cc
Density 8.14 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 65.265.2Oil Quenched from 1218°C
 65.665.6Oil Quenched from 1177°C
 65.865.8Oil Quenched from 1149°C
Modulus of Elasticity 207 GPa30000 ksi
Machinability 50 - 60 %50 - 60 %1% Carbon Steel
Izod Impact Unnotched 29.8 J22.0 ft-lbOil Quenched at 1177°C; 520°C Temper Temperature
 30.5 J22.5 ft-lbOil Quenched at 1204°C; 580°C Temper Temperature
 30.5 J22.5 ft-lbOil Quenched at 1204°C; 650°C Temper Temperature
 32.5 J24.0 ft-lbOil Quenched at 1204°C; 482°C Temper Temperature
 37.3 J27.5 ft-lbOil Quenched at 1177°C; 650°C Temper Temperature
 43.4 J32.0 ft-lbOil Quenched at 1177°C; 482°C Temper Temperature
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.95 µm/m-°C
@Temperature 21.0 - 204 °C
6.083 µin/in-°F
@Temperature 69.8 - 399 °F
 12.54 µm/m-°C
@Temperature 21.0 - 358 °C
6.967 µin/in-°F
@Temperature 69.8 - 676 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 830 °C1530 °FCritical Temperaure Ac1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.98 %0.98 %
Chromium, Cr 4.15 %4.15 %
Iron, Fe 81.29 %81.29 %
Manganese, Mn 0.28 %0.28 %
Molybdenum, Mo 5.0 %5.0 %
Silicon, Si 0.30 %0.30 %
Tungsten, W 6.15 %6.15 %
Vanadium, V 1.85 %1.85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Double Six™ ASTM M2 High Speed Steel
AISI Type A2 Tool Steel
Crucible Steel PM M2 Tool Steel
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)

NTIMK063 / 19410

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.