MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPV 3470N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 3470N is a high performance thermoplastic vulcanizate used in a variety of automotive, consumer and industrial applications. Sarlink TPV 3470N is a medium hardness, low density, RoHS compliant grade suitable for injection molding, blow molding and extrusion.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; General Purpose; Good Adhesion; High Heat Resistant; Low Density; Medium Hardness; Low Specific Gravity

Uses: Fittings; General Purpose; Piping; Potable Water Applications

RoHS Compliance: RoHS Compliant

Agency Ratings: NSF STD-61

Form: Pellets

Processing Method: Extrusion; Injection Molding; Blow Molding; Pipe Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Viscosity 290 cP
@Shear Rate 206 1/s,
Temperature 200 °C
290 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  71
@Time 5.00 sec
71
@Time 0.00139 hour
Extruded; ISO 868
 74
@Time 5.00 sec
74
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 5.20 MPa754 psiFlow; ASTM D412
 7.72 MPa1120 psiAcross Flow; ASTM D412
Tensile Strength, Yield 5.20 MPa754 psiFlow; ASTM D412
 7.72 MPa1120 psiAcross Flow; ASTM D412
Tensile Stress at Strain  3.10 MPa
@Strain 100 %
450 psi
@Strain 100 %
Across Flow; ISO 37
 3.81 MPa
@Strain 100 %
552 psi
@Strain 100 %
Flow; ISO 37
 3.26 MPa
@Strain 100 %,
Treatment Temp. 150 °C
473 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 3.41 MPa
@Strain 100 %,
Treatment Temp. 135 °C
495 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 380 %380 %Flow; ISO 37
 680 %680 %Across Flow; ISO 37
 585 %
@Treatment Temp. 150 °C,
Time 605000 sec
585 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 592 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
592 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tear Strength 42.1 kN/m240 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  25 %
@Temperature 22.8 °C,
Time 79200 sec
25 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 43 %
@Temperature 70.0 °C,
Time 79200 sec
43 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 47 %
@Temperature 125 °C,
Time 252000 sec
47 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 221 °C360 - 430 °FInjection
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Zone 1 182 - 204 °C360 - 400 °FExtrusion
Zone 2 182 - 204 °C360 - 400 °FExtrusion
Zone 3 188 - 210 °C370 - 410 °FExtrusion
Zone 4 188 - 210 °C370 - 410 °FExtrusion
Die Temperature 193 - 216 °C380 - 420 °FExtrusion
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® TPV X11059DB Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV 6765N Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV 2773 Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV 24545 Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV 22035N Thermoplastic Vulcanizate

PTEKNQ1149 / 237640

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.