MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Assab Steels Polmax Plastic Mold Material
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Excellent polishability. Good resistance to corrosion and wear. Good machinability.

Applications: Recommended where extreme surface finishes are required, such as lens moulds and CD moulds.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200hardness supplied.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 %0.38 %
Chromium, Cr 13.6 %13.6 %
Iron, Fe 84.32 %84.32 %
Manganese, Mn 0.50 %0.50 %
Silicon, Si 0.90 %0.90 %
Vanadium, V 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Assab Steels PRODAX Aluminum Alloy for Plastic Molds
Thermal Ceramics Kao-Plas C65 Plastic Monolithics
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Silicone Rubber
International Mold Steel P20 Plastic Mold Steel

NASSAB25 / 15043

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.