MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ineos L10G-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: L10G-00 is a barefoot polypropylene impact copolymer designed for injection molding applications. It offers excellent impact resistance, high flexural modulus and good processability. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

Applications

  • Injection molding
  • Consumer products
Benefits
  • High impact resistance
  • High flexural modulus

Information provided by Ineos Olefins & Polymers USA

Key Words: Excellent impact resistance, high flexural modulus and good processability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.908 g/cc0.0328 lb/in³ASTM D792
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090Injection Molded; ASTM D785
Tensile Strength at Break 15.4 MPa2240 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 26.7 MPa3870 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 250 %250 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 7.0 %7.0 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 1190 MPa172000 psiInjection Molded; ASTM D790A
Izod Impact, Notched  0.427 J/cm
@Temperature -20.0 °C
0.800 ft-lb/in
@Temperature -4.00 °F
Injection Molded; ASTM D256
 1.33 J/cm
@Temperature 22.8 °C
2.50 ft-lb/in
@Temperature 73.0 °F
Injection Molded; ASTM D256
Izod Impact, Notched (ISO)  4.39 kJ/m²
@Temperature -20.0 °C
2.09 ft-lb/in²
@Temperature -4.00 °F
Area, Injection Molded; ASTM D256
 12.9 kJ/m²
@Temperature 22.8 °C
6.14 ft-lb/in²
@Temperature 73.0 °F
Area, Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.8 °C199 °FUnannealed, Injection Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C125 °FUnannealed, Injection Molded; ASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 83 %83 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos N00G-01 Polypropylene Impact Copolymer
Ineos N00GX11 Polypropylene Impact Copolymer
Ineos N00M-00 Polypropylene Impact Copolymer
Ineos N01G-02 Polypropylene Impact Copolymer
Ineos N01N-00 Polypropylene Impact Copolymer

PINEOS912 / 130371

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.