MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos N00G-01 Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impact copolymers.

Key Words: Good impact and stiffness; Processability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.904 g/cc0.0327 lb/in³ASTM D792
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8282ASTM D785
Tensile Strength at Break 33.8 MPa4900 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 24.1 MPa3500 psi2.0 in/min; ASTM D638
Elongation at Break 900 %900 %2.0 in/min; ASTM D638
Elongation at Yield 10 %10 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1140 MPa165000 psiASTM D790A
Izod Impact, Notched  1.39 J/cm
@Temperature -20.0 °C
2.60 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO)  13.7 kJ/m²
@Temperature -20.0 °C
6.52 ft-lb/in²
@Temperature -4.00 °F
Area; ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.2 °C198 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C135 °FUnannealed; ASTM D648
Vicat Softening Point 153 °C307 °FASTM D1525
Brittleness Temperature <= -50.0 °C<= -58.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Gloss 56 %56 %60°; ASTM D2457
 
Descriptive Properties
ProcessInjection Molding
 Pipe Extrusion
 Sheet Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos N00M-00 Polypropylene Impact Copolymer
Ineos N01N-00 Polypropylene Impact Copolymer
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N00GX11 Polypropylene Impact Copolymer
Ineos N01G-02 Polypropylene Impact Copolymer

PINEOS919 / 171734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.