MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sandvik Kanthal Thermothal N Thermocouple wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Thermothal N is an austenitic nickel alloy (Ni alloy) used for the negative leg of thermocouples type K. Thermocouples type K have a good resistance to oxidation and better than other combinations of thermocouples. Thermothal N can not be exposed to atmospheres containing sulphur gases

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.60 g/cc0.311 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 120
@Diameter 2.00 mm
120
@Diameter 0.0787 in
Tensile Strength, Ultimate  481 MPa
@Temperature 500 °C
69800 psi
@Temperature 932 °F
 551 MPa
@Temperature 300 °C
79900 psi
@Temperature 572 °F
 563 MPa
@Temperature 100 °C
81700 psi
@Temperature 212 °F
 550 MPa
@Thickness 2.00 mm
79800 psi
@Thickness 0.0787 in
Tensile Strength, Yield  203 MPa
@Temperature 500 °C
29400 psi
@Temperature 932 °F
 224 MPa
@Temperature 300 °C
32500 psi
@Temperature 572 °F
 253 MPa
@Temperature 100 °C
36700 psi
@Temperature 212 °F
 250 MPa
@Strain 0.2 %,
Thickness 2.00 mm
36300 psi
@Strain 0.2 %,
Thickness 0.0787 in
Elongation at Break  36 %
@Temperature 300 °C
36 %
@Temperature 572 °F
 41 %
@Temperature 500 °C
41 %
@Temperature 932 °F
 42 %
@Temperature 100 °C
42 %
@Temperature 212 °F
 35 %
@Thickness 2.00 mm
35 %
@Thickness 0.0787 in
Modulus of Elasticity  42.0 GPa
@Temperature 500 °C
6090 ksi
@Temperature 932 °F
Young's
 61.0 GPa
@Temperature 300 °C
8850 ksi
@Temperature 572 °F
Young's
 91.0 GPa
@Temperature 100 °C
13200 ksi
@Temperature 212 °F
Young's
 194 GPa
@Temperature 20.0 °C
28100 ksi
@Temperature 68.0 °F
Young's
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000292 ohm-cm0.0000292 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.523 J/g-°C0.125 BTU/lb-°F
Thermal Conductivity 29.7 W/m-K
@Temperature 100 °C
206 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point 1400 °C2550 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.5 %1.5 %
Cobalt, Co 0.50 %0.50 %
Manganese, Mn 1.5 %1.5 %
Nickel, Ni 95 %95 %As Balance
Silicon, Si 1.5 %1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std
Hoskins Manufacturing Chromel® Thermocouple Wire
Constantan Thermocouple Wire
Sandvik Kanthal Nicrosil Thermocouple wire

NSANDV5045 / 199609

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.