MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik Kanthal Thermothal N Thermocouple wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Thermothal N is an austenitic nickel alloy (Ni alloy) used for the negative leg of thermocouples type K. Thermocouples type K have a good resistance to oxidation and better than other combinations of thermocouples. Thermothal N can not be exposed to atmospheres containing sulphur gases

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 120
@Diameter 2.00 mm
Tensile Strength, Ultimate 481 MPa
@Temperature 500 °C
 551 MPa
@Temperature 300 °C
 563 MPa
@Temperature 100 °C
 550 MPa
@Thickness 2.00 mm
Tensile Strength, Yield 203 MPa
@Temperature 500 °C
 224 MPa
@Temperature 300 °C
 253 MPa
@Temperature 100 °C
 250 MPa
@Strain 0.2 %,
Thickness 2.00 mm
Elongation at Break 36 %
@Temperature 300 °C
 41 %
@Temperature 500 °C
 42 %
@Temperature 100 °C
 35 %
@Thickness 2.00 mm
Modulus of Elasticity 42.0 GPa
@Temperature 500 °C
Young's
 61.0 GPa
@Temperature 300 °C
Young's
 91.0 GPa
@Temperature 100 °C
Young's
 194 GPa
@Temperature 20.0 °C
Young's
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000292 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.523 J/g-°C
Thermal Conductivity 29.7 W/m-K
@Temperature 100 °C
Melting Point 1400 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.5 %
Cobalt, Co 0.50 %
Manganese, Mn 1.5 %
Nickel, Ni 95 %As Balance
Silicon, Si 1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std
Hoskins Manufacturing Chromel® Thermocouple Wire
Constantan Thermocouple Wire
Sandvik Kanthal Nicrosil Thermocouple wire

NSANDV5045 / 199609

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.