MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asian Keruing, Apitong, Gurjun, Yang Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Liable to resin exudation
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Large/medium
Resistance to fungal decay (Heartwood in ground contact): Moderately Durable (10 to 15 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Heavy and general construction. Decking, vehicle flooring

Key Words: Dipterocarpus spp.; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.690 g/cc0.690 g/ccGreen
Density 0.740 g/cc0.0267 lb/in³15% Moisture Content. Density can vary by 20% or more.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4700 N1060 lb (f)Side Hardness, Green
 5600 N1260 lb (f)Side Hardness, 12% Moisture
Modulus of Rupture 0.0820 GPa11.9 ksiStatic Bending, Green
 0.1372 GPa19.90 ksiStatic Bending, 12% Moisture
Flexural Modulus 11.8 GPa1710 ksiStatic Bending, Green
 14.3 GPa2070 ksiStatic Bending, 12% Moisture
Compressive Strength 39.2 MPa5690 psiParallel to Grain, Green
 72.4 MPa10500 psiParallel to Grain, 12% Moisture
Machinability 10 %10 %Difficult Relative to Other Wood
Shear Strength 8.10 MPa1170 psiParallel to Grain, Green
 14.3 MPa2070 psiParallel to Grain, 12% Moisture
Work to Maximum Load 0.0960 J/cm³13.9 in-lb/in³Static Bending, Green
 0.162 J/cm³23.5 in-lb/in³Static Bending, 12% Moisture
 
Thermal PropertiesMetricEnglishComments
Shrinkage 5.2 %5.2 %Radial Shrinkage Green to Oven Dry
 5.2 %5.2 %Radial Shrinkage Green to Oven Dry
 10.9 %10.9 %Tangential Shrinkage Green to Oven Dry
 10.9 %10.9 %Tangential Shrinkage Green to Oven Dry
 16.1 %16.1 %Volumetric Shrinkage Green to Oven Dry
 16.1 %16.1 %Volumetric Shrinkage Green to Oven Dry
 
Descriptive Properties
ColorPinkish-brown to dark brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American White Oak Wood
Tropical Light Red Meranti Wood
Bur White Oak Wood
African Ekki/azobe Wood
Asian Kempas Wood

PTST410 / 71423

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.