MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Constellium Alumold® 400 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds and injection moulds for small series.

Information provided by manufacturer

Key Words: IS 5626
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.79 g/cc0.101 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  120
@Thickness 254 - 305 mm
120
@Thickness 10.0 - 12.0 in
 125
@Thickness 152.4 - 203.2 mm
125
@Thickness 6.000 - 8.000 in
 125
@Thickness 203.2 - 254 mm
125
@Thickness 8.000 - 10.0 in
 130
@Thickness 38.1 - 76.2 mm
130
@Thickness 1.50 - 3.00 in
 130
@Thickness 76.2 - 127 mm
130
@Thickness 3.00 - 5.00 in
 130
@Thickness 127 - 152.4 mm
130
@Thickness 5.00 - 6.000 in
 140
@Thickness 15.0 - 38.1 mm
140
@Thickness 0.591 - 1.50 in
Tensile Strength  >= 390 MPa
@Thickness 203.2 - 254 mm
>= 56600 psi
@Thickness 8.000 - 10.0 in
Tempers T651 / T652
 >= 395 MPa
@Thickness 152.4 - 203.2 mm
>= 57300 psi
@Thickness 6.000 - 8.000 in
Tempers T651 / T652
 >= 400 MPa
@Thickness 127 - 152.4 mm
>= 58000 psi
@Thickness 5.00 - 6.000 in
Tempers T651 / T652
 400 MPa
@Thickness 254 - 305 mm
58000 psi
@Thickness 10.0 - 12.0 in
Typical Strength
 >= 415 MPa
@Thickness 38.1 - 76.2 mm
>= 60200 psi
@Thickness 1.50 - 3.00 in
Tempers T651 / T652
 >= 415 MPa
@Thickness 76.2 - 127 mm
>= 60200 psi
@Thickness 3.00 - 5.00 in
Tempers T651 / T652
 420 MPa
@Thickness 203.2 - 254 mm
60900 psi
@Thickness 8.000 - 10.0 in
Typical Strength
 425 MPa
@Thickness 152.4 - 203.2 mm
61600 psi
@Thickness 6.000 - 8.000 in
Typical Strength
 >= 425 MPa
@Thickness 15.0 - 38.1 mm
>= 61600 psi
@Thickness 0.591 - 1.50 in
Tempers T651 / T652
 430 MPa
@Thickness 127 - 152.4 mm
62400 psi
@Thickness 5.00 - 6.000 in
Typical Strength
 440 MPa
@Thickness 38.1 - 76.2 mm
63800 psi
@Thickness 1.50 - 3.00 in
Typical Strength
 440 MPa
@Thickness 76.2 - 127 mm
63800 psi
@Thickness 3.00 - 5.00 in
Typical Strength
 450 MPa
@Thickness 15.0 - 38.1 mm
65300 psi
@Thickness 0.591 - 1.50 in
Typical Strength
Tensile Strength, Yield  >= 330 MPa
@Strain 0.2 %,
Thickness 203.2 - 254 mm
>= 47900 psi
@Strain 0.2 %,
Thickness 8.000 - 10.0 in
Tempers T651 / T652
 >= 340 MPa
@Strain 0.2 %,
Thickness 152.4 - 203.2 mm
>= 49300 psi
@Strain 0.2 %,
Thickness 6.000 - 8.000 in
Tempers T651 / T652
 340 MPa
@Strain 0.2 %,
Thickness 254 - 305 mm
49300 psi
@Strain 0.2 %,
Thickness 10.0 - 12.0 in
Typical Strength
 >= 350 MPa
@Strain 0.2 %,
Thickness 127 - 152.4 mm
>= 50800 psi
@Strain 0.2 %,
Thickness 5.00 - 6.000 in
Tempers T651 / T652
 360 MPa
@Strain 0.2 %,
Thickness 203.2 - 254 mm
52200 psi
@Strain 0.2 %,
Thickness 8.000 - 10.0 in
Typical Strength
 370 MPa
@Strain 0.2 %,
Thickness 152.4 - 203.2 mm
53700 psi
@Strain 0.2 %,
Thickness 6.000 - 8.000 in
Typical Strength
 >= 370 MPa
@Strain 0.2 %,
Thickness 38.1 - 76.2 mm
>= 53700 psi
@Strain 0.2 %,
Thickness 1.50 - 3.00 in
Tempers T651 / T652
 >= 370 MPa
@Strain 0.2 %,
Thickness 76.2 - 127 mm
>= 53700 psi
@Strain 0.2 %,
Thickness 3.00 - 5.00 in
Tempers T651 / T652
 >= 380 MPa
@Strain 0.2 %,
Thickness 15.0 - 38.1 mm
>= 55100 psi
@Strain 0.2 %,
Thickness 0.591 - 1.50 in
Tempers T651 / T652
 380 MPa
@Strain 0.2 %,
Thickness 127 - 152.4 mm
55100 psi
@Strain 0.2 %,
Thickness 5.00 - 6.000 in
Typical Strength
 395 MPa
@Strain 0.2 %,
Thickness 38.1 - 76.2 mm
57300 psi
@Strain 0.2 %,
Thickness 1.50 - 3.00 in
Typical Strength
 395 MPa
@Strain 0.2 %,
Thickness 76.2 - 127 mm
57300 psi
@Strain 0.2 %,
Thickness 3.00 - 5.00 in
Typical Strength
 410 MPa
@Strain 0.2 %,
Thickness 15.0 - 38.1 mm
59500 psi
@Strain 0.2 %,
Thickness 0.591 - 1.50 in
Typical Strength
Elongation at Break  5.0 %
@Thickness 254 - 305 mm
5.0 %
@Thickness 10.0 - 12.0 in
Typical Elongation
 >= 5.0 %
@Thickness 203.2 - 254 mm
>= 5.0 %
@Thickness 8.000 - 10.0 in
Tempers T651 / T652
 >= 6.0 %
@Thickness 152.4 - 203.2 mm
>= 6.0 %
@Thickness 6.000 - 8.000 in
Tempers T651 / T652
 >= 7.0 %
@Thickness 76.2 - 127 mm
>= 7.0 %
@Thickness 3.00 - 5.00 in
Tempers T651 / T652
 >= 7.0 %
@Thickness 127 - 152.4 mm
>= 7.0 %
@Thickness 5.00 - 6.000 in
Tempers T651 / T652
 >= 8.0 %
@Thickness 38.1 - 76.2 mm
>= 8.0 %
@Thickness 1.50 - 3.00 in
Tempers T651 / T652
 >= 9.0 %
@Thickness 15.0 - 38.1 mm
>= 9.0 %
@Thickness 0.591 - 1.50 in
Tempers T651 / T652
 9.0 %
@Thickness 152.4 - 203.2 mm
9.0 %
@Thickness 6.000 - 8.000 in
Typical Elongation
 9.0 %
@Thickness 203.2 - 254 mm
9.0 %
@Thickness 8.000 - 10.0 in
Typical Elongation
 10 %
@Thickness 76.2 - 127 mm
10 %
@Thickness 3.00 - 5.00 in
Typical Elongation
 10 %
@Thickness 127 - 152.4 mm
10 %
@Thickness 5.00 - 6.000 in
Typical Elongation
 11 %
@Thickness 38.1 - 76.2 mm
11 %
@Thickness 1.50 - 3.00 in
Typical Elongation
 12 %
@Thickness 15.0 - 38.1 mm
12 %
@Thickness 0.591 - 1.50 in
Typical Elongation
Modulus of Elasticity 73.0 GPa10600 ksicompression
Tensile Modulus 72.0 GPa10400 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.960 J/g-°C0.229 BTU/lb-°F
Thermal Conductivity 122 W/m-K847 BTU-in/hr-ft²-°F
 
Descriptive Properties
Thermal Diffusivity45.5 mm²/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Constellium Alumold® 350 Aluminum
Aluminum 7075-T73; 7075-T735x
Constellium Alumold® 500 Rolled Aluminum
MetalTek Nitronic® 33 Austenitic Stainless Steel
Superior Die Set FORTAL® HR Aluminum Alloy

NCONS013 / 160276

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.