MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Superior Die Set FORTAL® HR Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and doesn't require a very high ratio of resistance/mass. FORTAL offers machinability, high resistance to corrosion, and leads to increased productivity. FORTAL's modulus of elasticity is one third that of steel, and can absorb three times as much shock and vibration in its elastic phase. FORTAL is solution heat-treated, stabilized, artificially aged and stress relieved by stretching.

Application: FORTAL is an ideal material for all types of products and tooling since it is stronger than 1020 steels.

Information provided by Superior Die Set.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.77 g/cc0.100 lb/in³
Thickness 14000 - 92000 microns551 - 3620 milintermediate sizes also available
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 145145
 150150
Tensile Strength, Ultimate 540.0 MPa78320 psi
Tensile Strength, Yield 480 MPa69600 psi
Elongation at Break 10 %10 %
Modulus of Elasticity 71.98 GPa10440 ksi
Fatigue Strength  80.0 MPa
@# of Cycles 1.00e+8
11600 psi
@# of Cycles 1.00e+8
test bar (22mm diam.) notched (Kt = 3)
 160 MPa
@# of Cycles 1.00e+8
23200 psi
@# of Cycles 1.00e+8
test bar (22mm diam.) unnotched (Kt =1)
Shear Strength 331 MPa48000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.49 µm/m-°C
@Temperature 20.0 - 100 °C
13.05 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.958 J/g-°C0.229 BTU/lb-°F
Thermal Conductivity 130 W/m-K902 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 60.0 °C140 °FRecommended
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.07 %90.07 %
Chromium, Cr 0.23 %0.23 %
Copper, Cu 1.6 %1.6 %
Magnesium, Mg 2.5 %2.5 %
Zinc, Zn 5.6 %5.6 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Superior Die Set FORTAL® HP Aluminum Alloy
Constellium Fortal® Aluminum Alloy
Aluminum 7075-T6; 7075-T651
RSP Technology RSA-501 AE Aluminum Scandium Super Alloy (Scalmalloy)
Overview of materials for Aluminum Alloy

NSUP01 / 19247

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.