MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omya OMYAFIL® Calcium Carbonate
Categories: Ceramic

Material Notes: An ultrafine ground calcium carbonate for paper and board filling.

Information supplied by Omya North America.

Key Words: CaCO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 72 %72 %Slurry Solids
Brightness 96.5 %96.5 %T534 om-76 Brightness (Diffuse Reflectance)
Loss On Ignition  0.00 %
@Temperature 400 °C
0.00 %
@Temperature 752 °F
 42.6 %
@Temperature 900 °C
42.6 %
@Temperature 1650 °F
Particle Size 0.70 µm0.70 µmMedian Diameter
Specific Surface Area 11.5 m²/g11.5 m²/g
Brookfield Viscosity 200 cP
@Temperature 25.0 °C
200 cP
@Temperature 77.0 °F
No. 3 Spindle, 100 rpm
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 174.5, 176.170, 176.180
 
Descriptive Properties
Calcium Carbonate %98
Magnesium Carbonate %1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company VLF 80209 EM HS Nylon 6/6 (PA), Long Glass Fiber - Easy Molding - Heat Stabilized
Omya COVERCARB® 85 Calcium Carbonate
Omya OMYACARB® F - FL Calcium Carbonate
Omya SNOWHITE® 12-40 - PT Calcium Carbonate
Omya COVERCARB® HP Calcium Carbonate

EOMYA905 / 5617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.