MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company VLF 80209 EM HS Nylon 6/6 (PA), Long Glass Fiber - Easy Molding - Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.57 g/cc1.57 g/ccASTM D 792
Additive Loading 50 %50 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.17 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 259 MPa37500 psiASTM D 638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D 638
Tensile Modulus 15.9 GPa2300 ksiASTM D 638
Flexural Strength 400 MPa58000 psiASTM D 790
Flexural Modulus 15.2 GPa2200 ksiASTM D 790
Izod Impact, Notched 4.81 J/cm
@Thickness 3.17 mm
9.00 ft-lb/in
@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 14.9 J/cm
@Thickness 3.17 mm
28.0 ft-lb/in
@Thickness 0.125 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 271 - 299 °C520 - 570 °F
Mold Temperature 65.6 - 124 °C150 - 255 °F
Drying Temperature 79.4 °C
@Time 7200 - 14400 sec
175 °F
@Time 2.00 - 4.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 34.5 - 124 MPa5000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omya OMYAFIL® Calcium Carbonate
RTP Company RTP 4085 Polyphthalamide (PPA); Carbon Fiber
Avient OnForce™ LFT NN-60 LGF/000 Natural Nylon 66 with 60% Long Glass Fiber
Avient OnForce™ LFT NN-30 LCF/000 Natural Nylon 66 with 30% Long Carbon Fiber
Omya HYDROCARB® 90 HS Calcium Carbonate

PQZTA1450 / 159081

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.