MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Master Bond EP3HTSMed Silver Filled, Medical Grade Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond EP3HTSMed is a one component, silver filled, electrically conductive epoxy system featuring high shear strength and good temperature resistance along with a fast cure schedule. The epoxy system fully meets USP Class VI requirements. EP3HTSMed has conductivity; less than 1 millionth per cm. Typical curing schedules are 40-90 minutes at 250°F or 20-40 minutes at 300°F (minimum cure temperature is 235-240°F). Tensile shear strengths in excess of 1,000 psi are readily obtained using these fast cure times. EP3HTSMed requires no mixing prior to use and has a 6 month shelf life at room temperature when packaged in jars (syringes have a shelf life of 3 months). The service temperature range is -60°F to +400°F. It is 100% reactive and does not contain any solvents or volatiles. EP3HTSMed produces durable, high strength bonds which are resistant to severe thermal cycling and many chemicals including water, oil, fuels and most organic solvents. Its adhesion to metals, glass, ceramics, vulcanized rubbers and many plastics is excellent. The cured adhesive/sealant is a superior thermal and electrical conductor. Its color is silver. The convenient handling and rapid cure speed of EP3HTSMed makes it ideally suited for demanding manufacturing applications.

Product Advantages:

  • Single component system, no mixing prior to use
  • Easy application; contact pressure only required during cure; adhesive spreads evenly and smoothly
  • Rapid cure schedules, e.g. 20-40 minutes at 300°F or 40-90 minutes at 250°F
  • High tensile shear strength
  • Bonds well to a wide variety of substrates
  • Excellent thermal and electrical conductor
  • Ideal for rigorous manufacturing application
Key Features
  • USP Class VI certified
  • Exceptionally low volume resistivity
  • Serviceable from -60°F to +400°F
  • High shear strength
  • Unlimited working life at room temperature
  • Thixotropic paste

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.90 g/cc2.90 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 8060 - 80
Tensile Strength at Break >= 34.5 MPa>= 5000 psi
Shear Strength  >= 3.45 MPa
@Temperature 93.3 °C
>= 500 psi
@Temperature 200 °F
Tensile, Al to Al
 >= 6.89 MPa
@Temperature 23.9 °C
>= 1000 psi
@Temperature 75.0 °F
Tensile, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0010 ohm-cm<= 0.0010 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  20.0 - 40.0 min
@Temperature 149 °C
0.333 - 0.667 hour
@Temperature 300 °F
 40.0 - 90.0 min
@Temperature 121 °C
0.667 - 1.50 hour
@Temperature 250 °F
Shelf Life 3.00 - 6.00 Month
@Temperature 23.9 °C
3.00 - 6.00 Month
@Temperature 75.0 °F
in original unopened container
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Appearancesilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond UV15X-6MED-2 UV Curable Compound for Medical Applications
Master Bond UV15DC80Med One Component UV Curable Epoxy
Master Bond UV10TKMed One component UV curable, biocompatible, high viscosity compound
Master Bond UV10MED Biocompatible One Component UV Curable Adhesive System
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy

PMASTB392 / 149639

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.