MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Techmer ES Plastiblend® PC/ABS 1950
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Availability: North America

Forms: Pellets

Information provided by TP Composites, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Melt Flow  3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 7.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength, Yield 57.9 MPa8400 psiASTM D638
Elongation at Break 80 %80 %ASTM D638
Flexural Yield Strength 91.0 MPa13200 psiASTM D790
Flexural Modulus 2.48 GPa360 ksiASTM D790
Izod Impact, Notched 8.01 J/cm
@Thickness 3.17 mm
15.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C40.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Plastiblend® PC/ABS FR 1950 BK
LG Chemical LUPOY GP1000L PC, Transparent
Ashley Polymers Ashlene® P1043R Polycarbonate
Westlake Plastics Zelux® 20% GF Polycarbonate
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled

PTPC1206 / 137144

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.