MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Powder-coatable nylon 6.6 for injection molding, with conductive carbon black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Water Absorption 1.4 - 2.1 %1.4 - 2.1 %ISO 62
Water Absorption at Saturation 6.0 - 8.0 %6.0 - 8.0 %ISO 62
Viscosity Measurement 145145Viscosity index; ISO 307
Linear Mold Shrinkage 0.020 - 0.030 cm/cm0.020 - 0.030 in/inFRISETTA Test Method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 110 MPa16000 psiISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psiISO 527
Elongation at Break 5.0 %5.0 %ISO 527
Tensile Modulus 3.00 GPa435 ksiISO 527
Flexural Strength 65.0 MPa9430 psiISO 178
Flexural Modulus 2.70 GPa392 ksiISO 178
Charpy Impact Unnotched 3.60 J/cm²17.1 ft-lb/in²ISO 179/1eU
 3.70 J/cm²17.6 ft-lb/in²DIN 53453
 1.60 J/cm²
@Temperature -40.0 °C
7.61 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 2.90 J/cm²
@Temperature -30.0 °C
13.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 0.700 J/cm²3.33 ft-lb/in²DIN 53453
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °FISO 3146 DSC
Maximum Service Temperature, Air 150 °C302 °FContinuous; FRISETTA Test Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled
Nylene® 7250 C HS 50% Glass Fiber/Ceramic Reinforced, Low Warp, High Stiffness Specialty Nylon
Celanese Nilit FRIANYL A63 KG20 Nylon 6.6 for injection molding, 20% chalk filled
Celanese Nilit FRIANYL A63 H Nylon 6.6 for injection molding
Celanese Nilit FRIANYL A63 CV-CM 0830 9005/Z Powder-coatable nylon 6.6 for injection molding, 8% carbon fiber reinforced, 30% ceramic filled

PFRI008 / 38929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.