Description: Nylene® 7250 C HS is a 50% glass fiber/ceramic reinforced, low warp, high stiffness specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |