MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allvac® Vasco® 13-8Mo Precipitation Hardening Steel, Heat Treatment: 927°C (1700°F) + Age
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: Data provided by Allvac.

Applications: Airframe structurals, missile components, valve parts, fasteners, chemical process equipment.

Key Words: Allvac, an Allegheny Teledyne Company; Maraging Steel, UNS S13800; AMS 5629. DMS 2100; ASTM A 564; PH 13-8 Mo, 13-8Mo, 13-8PH, 13-8 PH, 13/8 Mo, 13/8Mo, 13/8PH, 13/8 PH
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.72 g/cc0.279 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 411411Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 450450Estimated from Rockwell C value.
Hardness, Rockwell C 4444
Hardness, Vickers 430430Estimated from Rockwell C value.
Tensile Strength, Ultimate 1483 MPa215100 psi
Tensile Strength, Yield 1379 MPa
@Strain 0.2 %
200000 psi
@Strain 0.2 %
Elongation at Break >= 10 %>= 10 %
Reduction of Area >= 40 %>= 40 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.05 %1.05 %
Carbon, C 0.050 %0.050 %
Chromium, Cr 12.8 %12.8 %
Iron, Fe 76 %76 %as balance
Manganese, Mn 0.10 %0.10 %
Molybdenum, Mo 2.3 %2.3 %
Nickel, Ni 8.0 %8.0 %
Nitrogen, N 0.0050 %0.0050 %
Phosphorus, P 0.0050 %0.0050 %
Silicon, Si 0.050 %0.050 %
Sulfur, S 0.0040 %0.0040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition RH950
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H950
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H1000
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H1050
AISI Type S13800 Stainless Steel (PH 13-8 Mo) longitudinal properties, condition H1100

NALL79 / 14811

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.