Data provided by Allvac. Applications: Airframe structurals, missile components, valve parts, fasteners, chemical process equipment. |
Allvac, an Allegheny Teledyne Company; Maraging Steel, UNS S13800; AMS 5629. DMS 2100; ASTM A 564; PH 13-8 Mo, 13-8Mo, 13-8PH, 13-8 PH, 13/8 Mo, 13/8Mo, 13/8PH, 13/8 PH |