RA130E-6020 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and industrial applications. Specifications: DIN 8078; DIN 8077; and EN ISO 15874.Information provided by Borealis AG |