MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Flint Hills P5C4K-089 Random Copolymer Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Features: Good clarity. Product does not contain animal derived components. Phthalate-free

Applications: Cast Film

Information provided by Flint Hills Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9292ASTM D785
Tensile Strength, Yield 28.0 MPa4060 psiASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus 0.970 GPa141 ksiTangent; ASTM D790
Flexural Modulus, 1% Secant 930 MPa135000 psiASTM D790
Izod Impact, Notched 1.15 J/cm2.15 ft-lb/inASTM D256
Gardner Impact >= 36.2 J>= 26.7 ft-lbASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C192 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1520(c) 3.1a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills P5M2Z-012 Polypropylene Random Copolymer
Borealis RE420MO Polypropylene Random Copolymer, Transparent
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Braskem RP 347 Injection Molding Polypropylene
Braskem RP340R Injection Molding Polypropylene

PFLINT815 / 142627

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.