MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik ACEMATT® OP 278 Silica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Properties and applications: ACEMATT OP 278 is an organic matting agent based on Methylmethacrylate and Styrene(copolymer). Application benefits and achievable characteristics in films:
    low residual gloss
  • pleasant surface roughness
  • attractive surface structure
  • low coefficient of friction
Benefits during film processing:
  • low torque
  • acceleration of gelling
  • high elasticity of film preserved
ACEMATT OP 278 is a polymeric matting agent. Methylmethacrylate, Butylacrylate and Styrene are the raw material used to manufacture this copolymer. The particle size of the incorporated matting particle is about 7µm. At a concentration of 1.0% b.w., films are effectively matted. The resulting gloss is very low. The roughness results in a desired grip and appealing surface structure. This matting agent is especially recommended for films based on PVC, ABS and PUR. It can be compounded during the premix step.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 1.0 %1.0 %ISO 787-2
 
Descriptive Properties
Content0.005Free monomers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Optical Grade
Covestro Makrolon® OP sheet Polycarbonate
Versalis SINKRAL C253/m² ABS, Heat Stabilized
LyondellBasell Hostacom BB 1162 F/M D73078 Polypropylene, 22% Talc Filled
LyondellBasell Hostacom BB 1113 F BLACK Polypropylene, 25% Talc Filled

PEVONIM029 / 197233

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.