MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Overview of materials for Polycarbonate, Optical Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.40 g/cc0.0434 - 0.0506 lb/in³Average value: 1.21 g/cc Grade Count:68
 1.02 - 1.02 g/cc
@Temperature 280 - 280 °C
0.0368 - 0.0368 lb/in³
@Temperature 536 - 536 °F
Average value: 1.02 g/cc Grade Count:1
Water Absorption 0.130 - 0.300 %0.130 - 0.300 %Average value: 0.169 % Grade Count:30
Moisture Absorption at Equilibrium 0.120 - 0.340 %0.120 - 0.340 %Average value: 0.188 % Grade Count:24
Water Absorption at Saturation 0.150 - 0.350 %0.150 - 0.350 %Average value: 0.255 % Grade Count:9
Water Vapor Transmission 15.0 g/m²/day0.966 g/100 in²/dayAverage value: 15.0 g/m²/day Grade Count:3
Oxygen Transmission 67.0 - 2760 cc-mm/m²-24hr-atm170 - 7010 cc-mil/100 in²-24hr-atmAverage value: 1160 cc-mm/m²-24hr-atm Grade Count:3
Nitrogen Transmission 12.0 - 510 cc-mm/m²-24hr-atm30.5 - 1300 cc-mil/100 in²-24hr-atmAverage value: 214 cc-mm/m²-24hr-atm Grade Count:3
Carbon Dioxide Transmission 380 - 16900 cc-mm/m²-24hr-atm965 - 42900 cc-mil/100 in²-24hr-atmAverage value: 7030 cc-mm/m²-24hr-atm Grade Count:3
Thickness 180 - 12700 microns7.09 - 500 milAverage value: 4280 microns Grade Count:4
Linear Mold Shrinkage 0.00400 - 0.0100 cm/cm0.00400 - 0.0100 in/inAverage value: 0.00627 cm/cm Grade Count:41
Linear Mold Shrinkage, Transverse 0.00400 - 0.00750 cm/cm0.00400 - 0.00750 in/inAverage value: 0.00610 cm/cm Grade Count:21
Melt Flow 4.80 - 150 g/10 min4.80 - 150 g/10 minAverage value: 23.6 g/10 min Grade Count:55
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 50.0 - 72.050.0 - 72.0Average value: 63.6 Grade Count:21
Hardness, Rockwell R 118 - 121118 - 121Average value: 119 Grade Count:32
Ball Indentation Hardness 115 - 116 MPa16700 - 16800 psiAverage value: 116 MPa Grade Count:3
Tensile Strength, Ultimate 53.9 - 72.0 MPa7820 - 10400 psiAverage value: 67.1 MPa Grade Count:31
Tensile Strength, Yield 50.0 - 75.8 MPa7250 - 11000 psiAverage value: 62.6 MPa Grade Count:59
Elongation at Break 6.00 - 170 %6.00 - 170 %Average value: 102 % Grade Count:68
Elongation at Yield 5.40 - 120 %5.40 - 120 %Average value: 11.0 % Grade Count:23
Modulus of Elasticity 2.30 - 2.41 GPa334 - 350 ksiAverage value: 2.35 GPa Grade Count:25
Flexural Yield Strength 74.0 - 131 MPa10700 - 19000 psiAverage value: 92.1 MPa Grade Count:56
Flexural Modulus 2.06 - 3.52 GPa299 - 511 ksiAverage value: 2.34 GPa Grade Count:66
Flexural Strain at Yield 7.00 %7.00 %Average value: 7.00 % Grade Count:3
Izod Impact, Notched 1.07 - 9.70 J/cm2.00 - 18.2 ft-lb/inAverage value: 7.36 J/cm Grade Count:34
Izod Impact, Unnotched 7.85 - 5340 J/cm14.7 - 10000 ft-lb/inAverage value: 8.50 J/cm Grade Count:5
Izod Impact, Notched (ISO) 65.0 - 70.0 kJ/m²30.9 - 33.3 ft-lb/in²Average value: 66.3 kJ/m² Grade Count:12
 10.0 - 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
4.76 - 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 12.0 kJ/m² Grade Count:9
 15.0 - 15.0 kJ/m²
@Temperature -30.0 - -30.0 °C
7.14 - 7.14 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 12.0 kJ/m² Grade Count:3
 15.0 - 15.0 kJ/m²
@Thickness 3.00 - 3.20 mm
7.14 - 7.14 ft-lb/in²
@Thickness 0.118 - 0.126 in
Average value: 12.0 kJ/m² Grade Count:3
Charpy Impact Unnotched 1000 J/cm² - NB4760 ft-lb/in² - NBGrade Count:20
 999.9 J/cm² - NB
@Temperature -60.0 - -30.0 °C
4759 ft-lb/in² - NB
@Temperature -76.0 - -22.0 °F
Grade Count:13
Charpy Impact, Notched 0.700 - 9.00 J/cm²3.33 - 42.8 ft-lb/in²Average value: 5.05 J/cm² Grade Count:22
 1.40 - 1.40 J/cm²
@Temperature -30.0 - -30.0 °C
6.66 - 6.66 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.40 J/cm² Grade Count:3
 1.40 - 1.40 J/cm²
@Thickness 3.00 - 3.00 mm
6.66 - 6.66 ft-lb/in²
@Thickness 0.118 - 0.118 in
Average value: 1.40 J/cm² Grade Count:3
Puncture Energy 60.0 J44.3 ft-lbAverage value: 60.0 J Grade Count:3
 65.0 - 70.0 J
@Temperature -30.0 - -30.0 °C
47.9 - 51.6 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 66.7 J Grade Count:3
Tensile Creep Modulus, 1 hour 2200 MPa319000 psiAverage value: 2200 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 1900 MPa276000 psiAverage value: 1900 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+17 ohm-cm1.00e+14 - 1.00e+17 ohm-cmAverage value: 3.29e+16 ohm-cm Grade Count:18
Surface Resistance 1.00e+15 - 1.00e+16 ohm1.00e+15 - 1.00e+16 ohmAverage value: 5.73e+15 ohm Grade Count:11
Dielectric Constant 2.85 - 3.102.85 - 3.10Average value: 3.04 Grade Count:14
Dielectric Strength 15.0 - 34.0 kV/mm380 - 864 kV/inAverage value: 25.0 kV/mm Grade Count:18
Dissipation Factor 0.000500 - 0.01000.000500 - 0.0100Average value: 0.00526 Grade Count:14
Arc Resistance 30.0 - 120 sec30.0 - 120 secAverage value: 95.0 sec Grade Count:12
Comparative Tracking Index 125 - 400 V125 - 400 VAverage value: 273 V Grade Count:17
Hot Wire Ignition, HWI 15.0 - 60.0 sec15.0 - 60.0 secAverage value: 33.8 sec Grade Count:8
High Amp Arc Ignition, HAI 60.0 - 120 arcs60.0 - 120 arcsAverage value: 105 arcs Grade Count:8
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minAverage value: 115 mm/min Grade Count:8
 
Thermal PropertiesMetricEnglishComments
CTE, linear 56.0 - 70.2 µm/m-°C31.1 - 39.0 µin/in-°FAverage value: 66.3 µm/m-°C Grade Count:48
CTE, linear, Transverse to Flow 60.0 - 70.0 µm/m-°C33.3 - 38.9 µin/in-°FAverage value: 66.7 µm/m-°C Grade Count:19
Specific Heat Capacity 0.00117 - 1.70 J/g-°C0.000280 - 0.406 BTU/lb-°FAverage value: 0.265 J/g-°C Grade Count:11
Thermal Conductivity 0.173 - 2.80 W/m-K1.20 - 19.4 BTU-in/hr-ft²-°FAverage value: 0.365 W/m-K Grade Count:16
Maximum Service Temperature, Air 70.0 - 120 °C158 - 248 °FAverage value: 109 °C Grade Count:9
Hot Ball Pressure Test 135 - 137 °C275 - 279 °FAverage value: 136 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 127 - 146 °C261 - 295 °FAverage value: 139 °C Grade Count:35
Deflection Temperature at 1.8 MPa (264 psi) 117 - 143 °C243 - 289 °FAverage value: 129 °C Grade Count:67
Vicat Softening Point 143 - 157 °C289 - 315 °FAverage value: 149 °C Grade Count:22
Minimum Service Temperature, Air -55.0 - -40.0 °C-67.0 - -40.0 °FAverage value: -41.9 °C Grade Count:8
Glass Transition Temp, Tg 144 - 145 °C291 - 293 °FAverage value: 145 °C Grade Count:5
UL RTI, Electrical 75.0 - 130 °C167 - 266 °FAverage value: 105 °C Grade Count:24
UL RTI, Mechanical with Impact 75.0 - 125 °C167 - 257 °FAverage value: 99.6 °C Grade Count:24
UL RTI, Mechanical without Impact 75.0 - 130 °C167 - 266 °FAverage value: 105 °C Grade Count:24
Flammability, UL94 HB - V-0HB - V-0Grade Count:47
Flash Point 480 - 550 °C896 - 1020 °FAverage value: 515 °C Grade Count:3
Oxygen Index 26.0 - 28.0 %26.0 - 28.0 %Average value: 27.2 % Grade Count:5
Glow Wire Test 775 - 960 °C1430 - 1760 °FAverage value: 868 °C Grade Count:8
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.58 - 1.591.58 - 1.59Average value: 1.59 Grade Count:35
Haze 0.500 - 1.50 %0.500 - 1.50 %Average value: 0.940 % Grade Count:20
Transmission, Visible 0.100 - 91.0 %0.100 - 91.0 %Average value: 81.6 % Grade Count:49
Reflection Coefficient, Visible (0-1) 0.970 - 0.9750.970 - 0.975Average value: 0.973 Grade Count:4
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 254 - 332 °C490 - 630 °FAverage value: 284 °C Grade Count:18
Melt Temperature 240 - 350 °C464 - 662 °FAverage value: 283 °C Grade Count:43
Mold Temperature 49.0 - 121 °C120 - 250 °FAverage value: 88.2 °C Grade Count:39
Injection Velocity 200 mm/sec7.87 in/secAverage value: 200 mm/sec Grade Count:4
Drying Temperature 116 - 121 °C241 - 250 °FAverage value: 120 °C Grade Count:31
Moisture Content 0.0200 %0.0200 %Average value: 0.0200 % Grade Count:5
Injection Pressure 51.7 - 152 MPa7500 - 22000 psiAverage value: 100 MPa Grade Count:16
Cycle Time - Injection 1.00 - 2.50 sec1.00 - 2.50 secAverage value: 1.75 sec Grade Count:6
Cycle Time - Cooling 5.00 - 40.0 sec5.00 - 40.0 secAverage value: 22.5 sec Grade Count:6
Vent Depth 0.00200 - 0.00800 cm0.000787 - 0.00315 inAverage value: 0.00500 cm Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Molded
Overview of materials for Polycarbonate, Extruded
Overview of materials for Polycarbonate, UV Stabilized
Overview of materials for Polycarbonate, High Heat
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant

O3105 / 78124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.