System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
IRPC Polimaxx Polene 3342R Polypropylene Random Copolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Copolymer
Material Notes:
CHARACTERISTICS:
HIGH CLARITY, HIGH FLOW, GOOD PROCESSABILITY
APPLICATIONS:
INJECTION MOLDING FOR FOOD CONTAINERS, HOUSEWARES, CRATES
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Melt Flow
20
g/10 min
@Load 2.16 kg,
Temperature 230 °C
20
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
94
94
ASTM D785
Tensile Strength, Yield
30.0
MPa
4350
psi
ASTM D638
Elongation at Yield
35 %
35 %
ASTM D638
Flexural Modulus, 1% Secant
1080
MPa
157000
psi
ASTM D790
Izod Impact, Notched
0.380
J/cm
@Temperature 23.0 °C
0.712
ft-lb/in
@Temperature 73.4 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Heat Distortion Temperature
83.0
°C
181
°F
ASTM D648
Processing Properties
Metric
English
Comments
Processing Temperature
180
-
230
°C
356
-
446
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
IRPC Polimaxx Polene 3342M Polypropylene Random Copolymer
Epsilon Polymers RN-355 Polypropylene Random Copolymer
Dow R792-35RNA Polypropylene Random Copolymer Resin
Global PP-3375-RM Polypropylene Random Copolymer
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer
PIRPC093 / 84070
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.