MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
IRPC Polimaxx Polene 3342R Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: CHARACTERISTICS: HIGH CLARITY, HIGH FLOW, GOOD PROCESSABILITY

APPLICATIONS: INJECTION MOLDING FOR FOOD CONTAINERS, HOUSEWARES, CRATES

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ASTM D785
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Yield 35 %ASTM D638
Flexural Modulus, 1% Secant 1080 MPaASTM D790
Izod Impact, Notched 38.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 83.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IRPC Polimaxx Polene 3342M Polypropylene Random Copolymer
Epsilon Polymers RN-355 Polypropylene Random Copolymer
Dow R792-35RNA Polypropylene Random Copolymer Resin
Global PP-3375-RM Polypropylene Random Copolymer
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer

PIRPC093 / 84070

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.